Brand Name : Senphus
Model Number : C-4
Certification : ISO9001
Place of Origin : China
MOQ : TBD
Price : TBD
Payment Terms : T/T, D/P
Supply Ability : 30 Tons per day
Delivery Time : 7 days
Packaging Details : Packed with waterproof paper or weave bag, into pallets or wooden case. Special packaging requirements can also be accommodated.
Place of Orig : China
Type : Hastelloy
Density : 8.6 g/cm³
Melting range : 1335-1380 ℃
Tensile strength Rm : 690 N/mm²
Yield strengthRP 0.2 : 276 N/mm²
Elongation A5 : 40%
Brinell Hardness HB : ≤200
Hastelloy C-4 ( UNS N06455 ) super alloy metallographic stability and oxidation resistance
General Overview:
Hastelloy C-4 is a nickel-chromium-molybdenum alloy known for its exceptional resistance to a wide variety of chemical environments and its stability across a broad range of temperatures. It is specifically designed to resist corrosion in highly aggressive conditions, making it suitable for use in chemical processing, pollution control, and other demanding industrial applications.
Hastelloy C-4 offers excellent resistance to localized corrosion such as pitting and crevice corrosion, as well as resistance to stress corrosion cracking. It performs well in both oxidizing and reducing environments and is resistant to a wide range of acids, including sulfuric, hydrochloric, and nitric acids. The alloy maintains its mechanical properties and corrosion resistance across a wide range of temperatures, making it suitable for high-temperature applications up to approximately 1038°C (1900°F). Hastelloy C-4 can be readily fabricated using standard techniques, including welding, which retains its corrosion resistance after welding. The alloy's composition is designed to prevent the formation of grain-boundary precipitates in the weld heat-affected zone, ensuring it remains resistant to intergranular corrosion after welding.
Chemical Processing:
Pollution Control:
Nuclear Industry:
Pharmaceutical Industry:
Pulp and Paper Industry:
Chemical Composition Wt.% | % | Ni | Cr | Fe | C | Mn | Si | Mo | Ti | P | S |
Min | Bal. | 14 | 14 | ||||||||
Max | Bal. | 18 | 3 | 0.015 | 1.0 | 0.08 | 17 | 0.7 | 0.04 | 0.03 |
Physical Constants | Density(g/cm³) | 8.6 | |||||
Melting Range(℃) | 1335-1380 |
Minimum mechanical properties of alloy at room temperature | Typical mechanical properties | Tensile strength Rm N/mm² | Yield strength RP 0.2 N/mm² | Elongation A5 % | Brinell Hardness HB | |||||
Solution treatment | 690 | 276 | 40 | ≤200 |
![]() |
UNS N06455 Hastelloy C4 Wire Metallographic Stability Oxidation Resistance Images |